Our company is specializing in manufacturing a series of Cotton Linter Pulp used for production of Bank note/Bond paper. As a variety needs of different customers in specification of Beating degree (Canadian Standard Freeness), Folding Endurance, Whiteness, Fluorescence, Ash, Fibre Length, Tensile Breaking Length, Moisture, Grammage, etc. we adopt cotton and cotton linter as raw material, based on new style clean process art to produce different specifications bleaching "totally chlorine free" cotton linter pulp which without any influence on printability and anti-counterfeiting in security.Now, our company is the biggest supplier for three China National Bank-note Paper Factory. From the beginning of 2005, our Cotton Linter Pulp use for production of Bank note/Bond paper started to export to international market.Description: This product is used for various currency paper and bondpaper production.Model Number: CPT1-800Specifications:1) Folding strength: ≥800 double times2) Fluorescence: ≤1.5m2/kg3) Brightness: ≥80%4) Average fiber length: 2.8 - 3.3mm5) Big and middle dust: ≤1/kg6) Small dust: ≤40mm2/kg7) Weight: 650±100g/m2
Thanks for your mails.We specialize in produce cotton linter pulp.Main products:A series of Cotton Linter Pulp used for production of Bank note/Bond paper.A series of Cotton Linter Pulp used for produ
Used for the production of filter paper for liquid food, beer, medicine,and chemical analysis. As well as for automobile filter paper, andvarious special industrial application papers.Specifications:1
Specifications:1) Degree of polymerization: ≥2, 5502) Brightness: ≥85%3) Ash: ≤0.08%4) Alpha cellulose: ≥995) Fe: ≤10ppm6) Weight: 650Φ100g/m27) This model is used f
Specifications:1) Degree of polymerization: ≥1,3002) Brightness: ≥85%3) Ash: ≤0.08%4) Alpha cellulose: ≥995) Fe: ≤10ppm6) Weight: 650±100g/m27) This model is used fo
Specifications:1) Degree of polymerization: ≥2,2002) Brightness: ≥85%3) Ash: ≤0.08%;4) Alpha cellulose: ≥995) Fe: ≤10ppm6) Weight: 650±100g/m27) This model is used f
Used for production of viscose staple fiber.Specifications:1) Degree of polymerization: 500±202) Alpha cellulose: ≥93%3) Ash: ≤0.10%4) Brightness: ≥80%